Yan GAO;Tao LuanJiwei Peng;Tao Lv
. 2013, 44(14): 2092-2096.
Abstract (
)
Download PDF (
)
Knowledge map
Save
The quaternary SCR catalyst was prepared with anatase TiO2 as the support, V2O5 as the main active agent, WO3 and MoO3 as the active coagent. The deNOx efficiency, catalytic selectivity, thermo stability and microscopic characterization of this catalyst were studied. The results showed that the deNOx efficiency of this quaternary catalyst was higher than the ternary catalyst singly loading W or Mo at the same weight percent. W improved the deNOx efficiency at high temperature and inhibited the side reaction caused by Mo at the temperature above 400 °C, while Mo improved the deNOx efficiency at low temperature which made up for the lower deNOx efficiency of W at the temperature below 300 °C. The maximum deNOx efficiency of this quaternary catalyst was 99%, the temperature window (deNOx efficiency>80%) was 280~420 °C, and the SO2 oxidation in the range of 180~380 °C was zero. There were three weight loss peaks for the quaternary catalyst in the range of 0~1000 °C, crystal water evaporation at 100~130 °C, organic additive decomposition at 230~270 °C and inorganic salt decomposition at 500~530 °C. The microscopic characterization showed the particle of this catalyst was uniform and compact, the grain size was consistent with no apparent agglomeration and macro pore structure was complete.